ASME Section IX's grouping of base metals with similar welding behaviour, so one procedure or welder test covers every material in the group: P-No. 1 for carbon steel, P-No. 8 for austenitic stainless.

Pujan Motiwala · · Updated

It matters because it decides how many procedure and welder tests a shop needs: a qualification on one P-No. 1 carbon steel covers the others, but welding P-No. 1 to P-No. 8 stainless is a dissimilar joint needing its own procedure. Group numbers inside a P-number matter when impact testing applies.

Common materials in each group, with F-numbers and A-numbers for filler metals, are in P-numbers, F-numbers and A-numbers. The P-number on a WPS is only as good as the record of which plate is in which seam; see material traceability.